PHYSICAL PROPERTIES |
|
PROPERTY |
RESULT |
Color |
White |
Thickness |
10.2 mil (0.26 mm) |
Membrane Weight |
0.95 oz/yd² (289 g/m²) |
60" Roll Weight |
48 lbs (22 kg) |
30" Roll Weight |
25 lbs (11 kg) |
Roll Dimensions |
60" x 100' (1.5 m x 30.5 m) |
Roll Coverage |
60" 500 ft² (46.5 m²) gross |
Primer |
No Primer Required |
VOCs |
None |
Field Exposure Before Roof/Cladding Materials |
Roofs: 180 days |
Minimum Application Temperature |
20°F (-6.6°C) and rising |
Service Temperature |
minus 40°F (-40°C) - 270°F (132.2°C) |
Warranty |
20 year material warranty |
TESTING DATA |
||
PROPERTY |
STANDARD |
RESULT |
Strength |
||
Elongation |
ASTM D412 Standard Test Methods for Vulcanized Rubber and Thermoplastic Elastomers—Tension |
MD - 409% |
Tensile Strength |
ASTM D412 Standard Test Methods for Vulcanized Rubber and Thermoplastic Elastomers—Tension |
MD - 16.96 MPa (2460 psi) |
Dry Tensile Strength |
ASTM D882 Standard Test Method for Tensile Properties of Thin Plastic Sheeting |
MD - 3.85 N/mm (22 lbf/in) |
Elongation at Break |
ASTM D882 Standard Test Method for Tensile Properties of Thin Plastic Sheeting |
MD - 541% |
Dry Breaking Force (Grab method) MD ≥40 XMD ≥35 |
ASTM D5034 Standard Test Method for Breaking Strength and Elongation of Textile Fabrics (Grab Test) |
MD – 338 N (76 lbsf) |
Elongation at Break |
ASTM D5034 Standard Test Method for Breaking Strength and Elongation of Textile Fabrics (Grab Test) |
MD - 120% |
Minimum Puncture Resistance |
ASTM E154 Standard Test Methods for Water Vapor Retarders Used in Contact with Earth Under Concrete Slabs, on Walls, or as Ground Cover |
Deflection 5.84 cm (2.3") |
Cold Mandrel Bend Test |
AC38 Section 3.3.4 |
PASS |
Weathering Tests |
AC38 Section 4.1.2 UV Exposure |
PASS |
Wear Resistance | Wheelbarrow Testing | PASS |
Self Adhering Flashing | AAMA 711-13 Voluntary Specification for Self Adhering Flashing Used for Installation of Exterior Wall Fenestration Products | Compliant |
Water Vapor Transmittance |
||
Water Vapor Transmission Desiccant Method Procedure A 23°C (73.4°F) 0-50 %RH |
ASTM E96 Standard Test Methods for Water Vapor Transmission of Materials |
0.0173 Perm (grain/h•ft²•inchHg) @23°C 100%RH |
Water Vapor Transmission Using Modulated Infrared Sensor |
ASTM F1249 Standard Test Method for Water Vapor Transmission Rate Through Plastic Film and Sheeting Using a Modulated Infrared Sensor |
0.0193 Perm (grain/h•ft2•inchHg) 1.10 ng/Pa•s•m2 |
Water Ponding | ICC-ES AC48 Acceptance Criteria for Self-Adhered Roof Underlayments for use as IBarriers | PASS |
Air Resistance Testing |
||
Air Permeance |
ASTM E2178 @75 Pa Standard Test Method for Air Permeance of Building Materials |
0.00912 L/s•m² @ 75 Pa (0.0018 cfm/ft² @ 1.57 psf) |
Air Permeance |
CAN/ULC-S741-08 (2020) Standard for Air Barrier Materials |
PASS |
Air Leakage Rate |
CAN/ULC-S742-11 Standard for Air Barrier Assemblies |
Class A1
|
Water Resistance Testing |
||
Nail Sealability |
ASTM D1970 Standard Specification for Self-Adhering Polymer Modified Bituminous Sheet Materials Used as Steep Roofing Underlayment for Ice Dam Protection Section 7.9 referring to ASTM D7349 protocol 4 with modifications |
PASS |
Water Resistance (Control after Weathering) |
AATCC 127 Hydrostatic pressure test (550 mm water column for 5 hours), American Association of Textile Chemists and Colorists |
PASS |
Fire Testing |
||
Flame Spread Smoke Developed |
ASTM E84 Standard Test Method for Surface Burning Characteristics of Building Materials |
Flame Spread 5 (Class A) |
UL |
UL790 Test Method of Fire Tests for Roof Coverings, CAN/ULC-S107 |
PASS |
Surface Burning Characteristics | CAN/ULC-S102 Protective Underlayment, Permeable to Allow Drying, Provides an Air Barrier | Flame Spread Rating: 5 Smoke Developed Value: 15 |