pdf Product Data Sheet (PDF) (3.85 MB)
PHYSICAL PROPERTIES |
||
PROPERTY |
WrapShield RS 3mm |
WrapShield RS 7mm |
Color |
Beige Membrane/Black Matrix |
|
Thickness with Matrix |
4.4 mm |
7.2 mm |
Membrane Weight with Matrix |
504.4 g/m² (1.9 oz/ft²) |
580.1 g/m² (1.653 oz/ft²) |
Roll Weight |
22 lbs (10 kg) |
13 lbs (5.9 kg) |
Roll Dimensions gross |
29.5” x 75’ 184.4 sq.ft (.75m x 22.9m, 17.1m²) |
29.5” x 37.5’, 92.2 sq.ft. (.75m x 11.4m, 8.6m²) |
Roll Dimensions Net |
27.5" x 75' 171.9 sq.ft. (.7m x 22.9m, 16 m²) |
27.5" x 37.5', 85.9 sq.ft. (.7m x 11.4m, 8m²) |
Skid |
15 Rolls |
|
Primer |
No Primer Required |
|
VOCs |
None |
|
Exposure Before Permanent Cladding |
6 months, 180 days |
|
Minimum Application Temperature |
20°F (-6°C) |
|
Service Temperature |
-40°F (-40°C) 225°F (107°C |
|
Warranty |
20 year material warranty |
TESTING DATA |
||
PROPERTY |
STANDARD |
RESULT |
Strength |
||
Dry Tensile Strength ≥ 20 lbs/in |
ASTM D828 Standard Test Method for Tensile Properties of Paper and Paperboard Using Constant-Rate-of-Elongation Apparatus |
MD - 6.1 N/mm (34.8 lbs/in) |
Dry Breaking Force (Grab method) MD ≥40 XMD ≥35 |
ASTM D5034 Standard Test Method for Breaking Strength and Elongation of Textile Fabrics (Grab Test) |
MD – 391 N (88 lbf) CD – 369 N (83 lbf) |
Cold Mandrel Bend Test |
AC38 Section 3.3.4 |
Warp (Machine) Direction - No cracking Filling (Cross) Direction - No cracking |
Weathering Tests |
AC38 Section 4.1.2 UV Exposure AC38 Section 4.1.3 Accelerated Aging |
UV - No visual change UV & Accelerated - visibly lighter, no visible deterioration |
Water Vapor Transmittance |
||
Water Vapor Transmission Desiccant Method 24.4°C (76.0°F) 50 %RH |
ASTM E96 Standard Test Methods for Water Vapor Transmission of Materials |
14.7 Perm (grain/h•ft2•inchHg) 480 ng/Pa•s•m2 |
Water Vapor Transmission Water Method 24.4°C (76.0°F) 50 %RH |
ASTM E96 Standard Test Methods for Water Vapor Transmission of Materials |
20.5 Perm (grains/hr•ft2•inchHg) 1171 ng/Pa•s•m2 |
Water Vapor Transmission Dynamic Relative Humidity Measurement (23°C 50 %RH) |
ASTM E398 Standard Test Method for Water Vapor Transmission Rate of Sheet Materials Using Dynamic Relative Humidity Measurement |
21.95 Perm (grain/h•ft2•inchHg) 1255 ng/Pa•s•m2 |
Adhesion Testing |
||
90° Peel Adhesion |
AAMA 711 |
PASS |
Water Resistance Testing |
||
Nail Sealability |
ASTM D1970/ section 7.9 Standard Specification for Self-Adhering Polymer Modified Bituminous Sheet Materials Used as Steep Roofing Underlayment for Ice Dam Protection |
Pass - pdf Review Fastener Penetrations Technical Bulletin (2.20 MB) |
Water Resistance (Boat Test) |
ASTM D779 Standard Test Method for Water Resistance of Paper, Paperboard, and Other Sheet Materials by the Dry Indicator Method (Withdrawn 2011) |
Control - No leakage Weathered - No Leakage |
Water Resistance (Control after Weathering) |
AATCC 127 Hydrostatic pressure test (550 mm water column for 5 hours), American Association of Textile Chemists and Colorists |
Control - No leakage Weathered - No Leakage |
Fire Testing |
||
Flame Spread Smoke Developed |
ASTM E84 Standard Test Method for Surface Burning Characteristics of Building Materials |
Flame Spread 10 Smoke Developed 75 (Class A) |