| PROPERTY | STANDARD/TEST | RESULT | RESULT | RESULT |
|---|---|---|---|---|
| Tensile Strength |
ASTM D1682 |
Control |
Accelerated Aged MD – 107.0 lbf/inch (18.7 N/mm) XMD – 81.4 lbf/inch PASS |
UV Exposed MD – 97.3 lbf/inch (17.0 N/mm) XMD - 76.7 lbf/inch PASS |
|
Water Vapor Transmission and Permeance |
ASTM E96* |
406.3 g/m² 24hrs |
||
|
Water Ponding |
AC 48, Section 4.4 |
PASS | ||
| Accelarated Aging |
AC48, Section 4.7 |
PASS | ||
|
UV Exposure |
AC48, Section 4.8 |
PASS | ||
|
Liquid Water Transmission |
ASTM D4869 |
PASS | ||
|
Rupture Resistance |
ASTM D3462 |
PASS | ||
|
Pliability |
ASTM E48 |
PASS |
FIRE TESTING
| PROPERTY | STANDARD/TEST | RESULT |
|---|---|---|
| Flamespread Index | ASTM E-84 | 10 – Class A PASS |
| Smoke Development Index | ASTM E-84 | 35 – Class A PASS |
INDEPENDENT TESTING
| PROPERTY | STANDARD/TEST | RESULT |
|---|---|---|
| Nominal Thickness | Calibrated Deadweight Micrometer | 0.020 inch (0.51mm) |
| Basis Weight | Electronic Weight Scale | 5.01 oz/yd² (0.55 oz/ft²) 170g/m² |
Acceptance Criteria for Polypropylene Roof Underlayments AC 207 & Acceptance Criteria for Roof Underlayments for use in severe climate areas AC48. Tested in accordance with ICC-ES AC 48 and AC 207 criteria to meet UBC, IBC and IRC requirements for Roofing Underlayments.